Latest / Civil Engineering Made Simple / Concrete Pavement Repair Manuals of Practice
Transcript
- 0:00Speaker 1: Welcome to the deep dive, where we take complex, dense
- 0:03Speaker 1: source material and turn it into actionable, memorable knowledge. Today
- 0:07Speaker 1: we are all about pavement durability. We're diving into the
- 0:10Speaker 1: Strategic Highway Research Program or SHRP findings. Specifically, we're looking
- 0:15Speaker 1: at the concrete pavement Repair Manuals of Practice. That's SHRP
- 0:20Speaker 1: H three forty nine.
- 0:21Speaker 2: That's right. This is the foundational work by Evans, Romain
- 0:25Speaker 2: Patel and mojeb And honestly it's still the gold standard
- 0:28Speaker 2: even though it's from back in ninety three to ninety four.
- 0:31Speaker 1: And our mission for you is pretty simple. If you're
- 0:32Speaker 1: a civil engineering student, a young professional, you know, anyone
- 0:36Speaker 1: managing public assets. We're pulling out the most critical step
- 0:39Speaker 1: by step insights on two key things joint resealing and
- 0:43Speaker 1: partial depths bawl repair.
- 0:44Speaker 2: And it's so important to establish upfront. This isn't just
- 0:46Speaker 2: textbook theory. I mean these manuals come from exhaustive literature reviews,
- 0:50Speaker 2: but also from the H one zero six field testing program.
- 0:52Speaker 2: They were out there at twenty two sites across the
- 0:54Speaker 2: US and Canada, so.
- 0:55Speaker 1: This is proven on the ground practice.
- 0:58Speaker 2: Exactly, these methods we're tested in all sorts of climates
- 1:01Speaker 2: and traffic conditions. This is the real playbook for successful repair.
- 1:05Speaker 1: Okay, so let's start with joint resealing. It feels like
- 1:08Speaker 1: the whole foundation of preventive maintenance is knowing when to
- 1:12Speaker 1: reseal a PCC joint. If you're too late, everything starts
- 1:16Speaker 1: falling apart.
- 1:17Speaker 2: It really is miss that window and water gets in,
- 1:20Speaker 2: and that just accelerates all kinds of deterioration.
- 1:23Speaker 1: So how do the manuals guide that decision. It can't
- 1:26Speaker 1: just be a visual check.
- 1:27Speaker 2: No, they force you to be quantitative. You start by
- 1:30Speaker 2: calculating what's called the sealant condition number or SCNF. It's
- 1:34Speaker 2: essentially a leak risk assessment. You look at two things. First,
- 1:37Speaker 2: what percentage of the joint length is actually letting water
- 1:40Speaker 2: get past the seal? And second, how bad is the
- 1:43Speaker 2: stone intrusion? Is it low, medium, or high?
- 1:46Speaker 1: And that gives you a number it does, and.
- 1:48Speaker 2: If your sen comes in between four and six, the
- 1:51Speaker 2: manual flags that seal as poor. Simple as that.
- 1:54Speaker 1: Okay, so that's the seal itself, But what about the
- 1:56Speaker 1: pavement around it? I assume that matters too.
- 1:58Speaker 2: It matters a lot. That's the next step you calculate
- 2:01Speaker 2: the pavement condition number, or PCN. This is all about
- 2:04Speaker 2: the structural damage that's already there.
- 2:06Speaker 1: What are the big indicators for the PCN?
- 2:08Speaker 2: You're looking for things like surface staining or pumping. That's
- 2:11Speaker 2: when you see water and fines getting ejected from under
- 2:14Speaker 2: the slab, big red flag for sub base erosion. You're
- 2:17Speaker 2: also looking for faulting. That's the little vertical drop off
- 2:20Speaker 2: between slabs and D cracking.
- 2:22Speaker 1: And for anyone listening who isn't looking at a diagram,
- 2:25Speaker 1: what does D cracking typically look like on the surface?
- 2:28Speaker 2: Good question. D cracking. You'll see these really closely spaced cracks,
- 2:33Speaker 2: almost like a web. They usually follow the joint lines
- 2:36Speaker 2: and are often filled with dark deposits. It's from freeze
- 2:39Speaker 2: though cycles in the aggregate itself.
- 2:41Speaker 1: So a high PCN is bad, very bad.
- 2:44Speaker 2: Specifically if you're in the six to fifteen range. The
- 2:47Speaker 2: pavement is officially rated as poor.
- 2:49Speaker 1: And of course you have to factor in climate. A
- 2:51Speaker 1: seal in Arizona is going to pave very differently than
- 2:53Speaker 1: one in say, Vermont.
- 2:55Speaker 2: Absolutely the manual breaks it down into four comatic regions.
- 2:58Speaker 2: It's all based on a twenty five annual precipitation threshold
- 3:02Speaker 2: and how many days you get below thirty two degrees fahrenheit,
- 3:05Speaker 2: which is easy wet freeze, wet non freeze, dry freeze,
- 3:07Speaker 2: and dry non freeze.
- 3:09Speaker 1: So you take the SCN, the PCN, the climate and traffic.
- 3:13Speaker 2: Levels and traffic level YEP low is under five thousand
- 3:17Speaker 2: vehicles a day, high is over thirty five thousand. You
- 3:21Speaker 2: plug all that into the decision table and the manual
- 3:24Speaker 2: and it gives you straight answer yes, possibly or no
- 3:28Speaker 2: on resealing. It takes out all the guesswork.
- 3:30Speaker 1: Okay, so let's say the answer is yes. Now we're
- 3:32Speaker 1: in the planning phase and this is where the real
- 3:35Speaker 1: engineering trade offs start.
- 3:36Speaker 2: Exactly. The first question is what's your goal A temporary
- 3:40Speaker 2: one to two year fix or long term solution that
- 3:43Speaker 2: lasts five plus years. That decision changes everything.
- 3:47Speaker 1: And there's an order of operations, right.
- 3:49Speaker 2: The critical one. Yeah, you must fix major defects first.
- 3:53Speaker 2: If you have full depth balls or need to do
- 3:55Speaker 2: under ciling for voids, that has to happen before you
- 3:58Speaker 2: even think about resealing the joint.
- 4:00Speaker 1: Then you get to the design of the seal itself.
- 4:02Speaker 1: The manual talks a lot about shape factor. Why is
- 4:04Speaker 1: that ratio so important?
- 4:05Speaker 2: The shape factor, that's the ratio of the ceilants width
- 4:08Speaker 2: to its thickness WTT And it's critical because these ceilants
- 4:12Speaker 2: are elastomers. They have to stretch and compress. If the
- 4:15Speaker 2: ceilant is too thick compared to its width, the strain
- 4:18Speaker 2: on the pond line where it sticks to the concrete
- 4:21Speaker 2: becomes huge when the joint opens in the cold, and
- 4:24Speaker 2: that's how it fails. It just rips away from the side.
- 4:26Speaker 1: So what's the recommended ratio?
- 4:28Speaker 2: It depends on the material. For something high performance like
- 4:31Speaker 2: a cold applied silicone, the recommendation is typically two to one.
- 4:35Speaker 2: For a less elastic material like rubberized asphalt, it's closer
- 4:39Speaker 2: to one to one.
- 4:39Speaker 1: And there are lots on thickness.
- 4:41Speaker 2: For silitone, there are a minimum of a quarter inch
- 4:44Speaker 2: and a maximum of a half inch.
- 4:45Speaker 1: This brings us to the elephant in the room. Cost.
- 4:49Speaker 1: The material prices are just worlds apart.
- 4:51Speaker 2: Oh yeah, it's a massive difference. Your hot applied rubberized
- 4:54Speaker 2: asphalt might be what two to four dollars a gallon,
- 4:57Speaker 2: but a self leveling silicone can be thirty to thirty
- 5:00Speaker 2: five dollars a gallon.
- 5:01Speaker 1: Wow, So is there a scenario where you can actually
- 5:04Speaker 1: justify that tenfold price increase?
- 5:06Speaker 2: Absolutely, especially in those extreme wet freeze climates. You're paying
- 5:11Speaker 2: for extension capacity. The rubberized asphalt might only handle fifteen
- 5:15Speaker 2: to thirty percent stretch before it fails. The silicones can
- 5:18Speaker 2: handle thirty to fifty percent. If you have huge thermal movements,
- 5:22Speaker 2: that expensive silicone is really your only viable long term option.
- 5:26Speaker 1: And there's another little piece of the puzzle that's easy
- 5:28Speaker 1: to overlook. The backer rod.
- 5:30Speaker 2: It's fundamental. People think it's just filler, but it is
- 5:33Speaker 2: two critical things. It controls the sealent thickness to get
- 5:37Speaker 2: that perfect shape factor, and it prevents the sealant from
- 5:40Speaker 2: bonding to the bottom of the joint.
- 5:41Speaker 1: It only bonds to the sides right.
- 5:43Speaker 2: Which allows it to stretch properly. And ship manual is
- 5:46Speaker 2: very clear the backer rod's diameter must be at least
- 5:49Speaker 2: twenty five percent larger than the joint with that ensures
- 5:52Speaker 2: itsts in place through compression.
- 5:54Speaker 1: That tiny twenty five percent difference sounds like the margin
- 5:57Speaker 1: between a five year repair and a one year failure. Okay,
- 6:01Speaker 1: let's move to construction. This is where a great design
- 6:03Speaker 1: can fall apart. Where do cruse most often get.
- 6:06Speaker 2: It wrong, Almost always in the prep sequence. The goal
- 6:09Speaker 2: is non negotiable, a clean, dry, properly dimension joint. If
- 6:15Speaker 2: those side walls have any dust, moisture or old residue,
- 6:18Speaker 2: the bond is doomed from the start.
- 6:20Speaker 1: So what's the gold standard sequence?
- 6:22Speaker 2: The best practice option one in the manual is a
- 6:25Speaker 2: multi stage process. First is prep. You plow out the
- 6:28Speaker 2: old stuff. Then you saw or reface the sidewalls with
- 6:32Speaker 2: water cooled diamond blades. That gives you a uniform surface
- 6:36Speaker 2: of fresh sound concrete.
- 6:38Speaker 1: But wait, water cooled blades that creates a slurry of concrete,
- 6:42Speaker 1: dust and water. Isn't that the absolute enemy of a
- 6:44Speaker 1: clean bond?
- 6:45Speaker 2: It is the absolute worst enemy, And that's the critical step.
- 6:48Speaker 2: You have to immediately and thoroughly remove that slurry. If
- 6:51Speaker 2: it dries on the side walls, it's like a permanent
- 6:53Speaker 2: bond inhibitor. Nothing will stick to it.
- 6:54Speaker 1: Okay, So after the wash, what's next? In the cleaning face?
- 6:57Speaker 2: This is the most crucial part. You follow up with
- 6:59Speaker 2: a brace of lasting sand blasting to roughen up and
- 7:02Speaker 2: deep clean those sidewalls. You need at least ninety psi
- 7:05Speaker 2: and the air has to be totally clean, dry and
- 7:07Speaker 2: oil free.
- 7:08Speaker 1: And you hold the nozzle right up close.
- 7:10Speaker 2: One to two inches from the surface. Then right after
- 7:13Speaker 2: that comes the final clean air blasting at least one
- 7:17Speaker 2: hundred psi. Again totally clean air. This blows out any
- 7:22Speaker 2: final dust from the sand blasting.
- 7:23Speaker 1: And I'm guessing the word immediately is key there.
- 7:25Speaker 2: It's everything. You don't want any ambient dust settling back
- 7:28Speaker 2: in the air. Blasting has to happen right before you
- 7:31Speaker 2: install the.
- 7:31Speaker 1: Backer rod, So then you move to installation.
- 7:34Speaker 2: Third stage yep primer if it's specified. Then the backer
- 7:39Speaker 2: rod goes in set to the perfect depth. And with
- 7:42Speaker 2: hot applied sealings, temperature control is everything. They have to
- 7:45Speaker 2: be poured in a very narrow range, like three seventy
- 7:48Speaker 2: to three ninety fahrenheit. You absolutely cannot cook them hold
- 7:51Speaker 2: them at that temperature for too long. Some materials have
- 7:53Speaker 2: a limit.
- 7:54Speaker 1: Of just six hours, and for the expensive cold applied silicon, you.
- 7:57Speaker 2: Have to make sure it's recessed exactly a quarter right
- 8:00Speaker 2: in below the pavement surface that protects it from trafficwaar
- 8:03Speaker 2: Let's circle.
- 8:03Speaker 1: Back to the high cost of silicone for a minute.
- 8:05Speaker 1: As an engineer, you have to justify that expense. How
- 8:08Speaker 1: do the manuals help us quantify that decision?
- 8:10Speaker 2: They push you to use a full cost effectiveness calculation,
- 8:14Speaker 2: usually based on average annual costs. And this is where
- 8:17Speaker 2: the expensive materials often.
- 8:19Speaker 1: Win because it's not just about material costs, not at all.
- 8:22Speaker 2: You have to include material, labor, equipment, And this is
- 8:26Speaker 2: the big one. User delay costs.
- 8:28Speaker 1: The cost of shutting down a lane, traffic jams, lost productivity.
- 8:31Speaker 2: Exactly on a busy highway, that delay cost can be
- 8:34Speaker 2: more than all the other costs combined. If a cheap
- 8:37Speaker 2: sealant only lasts three years, you have to shut down
- 8:40Speaker 2: that major lane every three years. The user delay costs
- 8:44Speaker 2: just become astronomical.
- 8:45Speaker 1: So the long term view changes the math completely.
- 8:48Speaker 2: It does. The SHRP manual had a sample calculation that
- 8:51Speaker 2: showed this perfectly. The high performance silicone had an average
- 8:55Speaker 2: annual cost of about twenty one hundred dollars per laye
- 8:57Speaker 2: mile because it lasted so long. The cheaper asphalt ceilant
- 9:01Speaker 2: was over twenty nine hundred dollars. Longevity is the tie breaker.
- 9:04Speaker 1: That's a perfect example of how engineering decisions have these
- 9:07Speaker 1: huge economic ripple effects. Okay, so what if you've missed
- 9:10Speaker 1: the joint ceiling window and now you have a spall
- 9:12Speaker 1: a chunk of concrete missing from the surface. Let's switch
- 9:15Speaker 1: to the second manual, partial depth spall repair.
- 9:18Speaker 2: Right. Spall repair is that next level of proactive maintenance,
- 9:23Speaker 2: and the first thing you need to know is the
- 9:24Speaker 2: strict depth limitation.
- 9:26Speaker 1: What causes a spall in the first place.
- 9:28Speaker 2: It's usually from incompressible material like little stones or sand
- 9:32Speaker 2: getting into a joint. When the slabs expand in the heat,
- 9:36Speaker 2: that debris gets trapped, the pressure builds and pop the
- 9:39Speaker 2: concrete surface breaks out. The rule for a partial depth
- 9:43Speaker 2: repair is that the damage is limited to the top
- 9:45Speaker 2: third of the slab and has to be at least
- 9:47Speaker 2: two inches deep to be stable.
- 9:49Speaker 1: And if it's deeper.
- 9:50Speaker 2: If it goes deeper than that top third, or if
- 9:52Speaker 2: you see any dowel bars or rebar, you have to stop.
- 9:55Speaker 2: It's no longer a partial depth repair. You must switch
- 9:57Speaker 2: to a full depth repair.
- 9:59Speaker 1: That's a critical decision point. So how do you verify
- 10:02Speaker 1: the extent of the damage before you start cutting.
- 10:04Speaker 2: You do it by sounding. You take a steel rod
- 10:06Speaker 2: or a hammer, and you tap the area around the
- 10:09Speaker 2: spall and.
- 10:09Speaker 1: You're listening for a change in pitch.
- 10:11Speaker 2: Exactly. Good sound concrete gives you a clear ringing sound.
- 10:16Speaker 2: Deteriorated weak concrete sounds dull, sort of the thud. That
- 10:20Speaker 2: dull sound tells you where the boundary of your repair
- 10:22Speaker 2: needs to be.
- 10:23Speaker 1: And what about the final dimensions of the patch.
- 10:26Speaker 2: The manuals recommend a minimum of four inches wide by
- 10:30Speaker 2: ten inches long, and you should always extend the patch
- 10:32Speaker 2: boundary about two to six inches beyond where you can
- 10:34Speaker 2: see the damage. That make sure you get all the
- 10:36Speaker 2: underlying weak material.
- 10:38Speaker 1: Okay, so we've defined the area and now we need
- 10:40Speaker 1: to fill it. We need fast setting materials. Here. What
- 10:42Speaker 1: are the main options?
- 10:43Speaker 2: They're three main categories. First, you have sementitious concretes. This
- 10:48Speaker 2: includes your high early strength Type three Portland cement mixes.
- 10:52Speaker 2: In warm weather, they can be ready for traffic in
- 10:55Speaker 2: just four to twelve hours, but you have to be
- 10:57Speaker 2: careful with some proprietary mixess like magnesium phosphate Set forty five.
- 11:02Speaker 2: They're super fast, but they're very sensitive to too much
- 11:05Speaker 2: water and they won't bond well. If you have limestone
- 11:08Speaker 2: aggregate in your existing pavement, an incompatibility issue a huge one.
- 11:12Speaker 2: Second category is polymer concretes. These are generally stronger and
- 11:16Speaker 2: set even faster. Epoxies are great, but you might have
- 11:19Speaker 2: to place them in thin layers or lifts to control
- 11:22Speaker 2: the heat they generate while curing. Methyl methacrylates are also great,
- 11:27Speaker 2: high strength, good working time, and then polyurethanes are interesting.
- 11:30Speaker 2: You often just preplace the dry aggregate in the hole
- 11:33Speaker 2: and then pour the liquid resin over it.
- 11:36Speaker 1: And the third category the quick and dirty option.
- 11:39Speaker 2: That would be your bituminous materials, things like a high
- 11:42Speaker 2: performance cold mix. It's very fast to place, but it's
- 11:45Speaker 2: really more of a temporary fix. It doesn't have the
- 11:47Speaker 2: long term durability of the other two.
- 11:49Speaker 1: Okay, let's talk about making the hole. The manual lists
- 11:52Speaker 1: a few methods for removing the bad concrete.
- 11:55Speaker 2: Right, and how you make that hole really affects how
- 11:57Speaker 2: well the patch will survive. The standard method is saw
- 12:00Speaker 2: and patch. It gives you nice vertical edges, which is
- 12:03Speaker 2: great structurally.
- 12:04Speaker 1: What's the downside.
- 12:05Speaker 2: The water from the saw means you have to wait
- 12:07Speaker 2: for things to dry, and you always have to create
- 12:09Speaker 2: an overcut sawing a bit beyond the boundary, which you
- 12:12Speaker 2: have to seal later.
- 12:13Speaker 1: What about just chipping it out?
- 12:14Speaker 2: That's chip and patch. The pro is you get a
- 12:17Speaker 2: really rough edge that helps with mechanical bonding. The con
- 12:22Speaker 2: is that it's very hard to avoid feathering the edges
- 12:24Speaker 2: where the patch gets really thin at the surface. That's
- 12:27Speaker 2: a major weak point. And for bigger jobs, for large areas,
- 12:31Speaker 2: you'd use millon patch. It's very efficient. The guide says
- 12:34Speaker 2: if you use this method, you should try to round
- 12:37Speaker 2: the patch edges that are parallel to traffic to reduce
- 12:40Speaker 2: the impact from tires.
- 12:42Speaker 1: Then there's the high tech option, water blasting.
- 12:44Speaker 2: The water blast and patch method, we're talking extremely high
- 12:47Speaker 2: pressure fifteen thousand to thirty thousand psi. The beauty of
- 12:50Speaker 2: it is that it only removes the weak concrete and
- 12:53Speaker 2: it leaves an incredibly rough surface, which is perfect for bonding.
- 12:57Speaker 1: But the cons are probably cost and water exactly high cost,
- 13:01Speaker 1: and it completely saturates the repair area, so you.
- 13:03Speaker 2: Have had a long drying delay before you can place
- 13:05Speaker 2: your patch material.
- 13:06Speaker 1: It seems like no matter how you remove the concrete,
- 13:08Speaker 1: the final cleaning step is absolutely nonagoable.
- 13:11Speaker 2: It is the key to adhesion. After removal, you have
- 13:15Speaker 2: to sand blast the cavity that roughens the surface and
- 13:18Speaker 2: gets rid of any final residue. Then, immediately after you
- 13:22Speaker 2: use high pressure air blasting again. It has to be
- 13:24Speaker 2: one hundred percent oil and water free to get all
- 13:27Speaker 2: the dust out.
- 13:27Speaker 1: And there's a test for cleanliness right the black glove test.
- 13:31Speaker 2: The inspector wipes the surface with a clean black glove.
- 13:34Speaker 2: If you see any dust on that glove, it's not
- 13:36Speaker 2: clean enough. You have to blast it again.
- 13:38Speaker 1: So before you place the new material, there's one more component,
- 13:41Speaker 1: the joint bond breaker.
- 13:43Speaker 2: Yes, this is critical. If you're using a rigid sementitious patch,
- 13:47Speaker 2: that patch can't handle the compression forces when the whole
- 13:50Speaker 2: slab expands. The bond breaker isolates the patch from those
- 13:54Speaker 2: forces right at the joint line.
- 13:55Speaker 1: What's it made of, usually a.
- 13:57Speaker 2: Non absorbent strip of polystyrene or polyethylene. You install it
- 14:01Speaker 2: slightly compressed and it should extend below and beyond the
- 14:03Speaker 2: patch boundaries. The best ones have a scored top layer
- 14:06Speaker 2: you can tear off later.
- 14:07Speaker 1: Which creates the reservoir for the new joint. Ceiland exactly.
- 14:11Speaker 2: It creates a perfect clean channel.
- 14:14Speaker 1: Okay, So placement and curing for these fast setting cements
- 14:17Speaker 1: you have to be precise.
- 14:19Speaker 2: You do use internal pencil vibrators to consolidate the material,
- 14:23Speaker 2: hold them at a shallow angle, maybe fifteen to thirty degrees,
- 14:26Speaker 2: and only move them vertically until all the air bubbles
- 14:29Speaker 2: stop rising. And in hot weather curing is critical. Use
- 14:33Speaker 2: a white pigmented curing compound. It reflects the sun's heat
- 14:37Speaker 2: and keeps the moisture in the patch so it can
- 14:39Speaker 2: gain strength properly.
- 14:41Speaker 1: And the final step is cealing that joint you created.
- 14:44Speaker 2: It is, but you have to wait. With non flexible materials,
- 14:47Speaker 2: you should generally let the patch cure for at least
- 14:50Speaker 2: a week before you seal the joint.
- 14:51Speaker 1: And the million dollar question for any road crew, when
- 14:54Speaker 1: can we open the lane to traffic?
- 14:56Speaker 2: You can open it as soon as the concrete hits
- 14:58Speaker 2: its minimum required of strength, And because this is a
- 15:02Speaker 2: shallow repair that's confined by the surrounding slab, that strength
- 15:05Speaker 2: requirement is often lower than the typical twenty eight day strength,
- 15:08Speaker 2: so you can get back in service pretty quickly.
- 15:10Speaker 1: That was an incredibly comprehensive journey. We went from diagnostics
- 15:14Speaker 1: using SCN and PCN to the geometry of shape factors,
- 15:18Speaker 1: all the way to the zero tolerance procedures for actually
- 15:20Speaker 1: building these repairs.
- 15:21Speaker 2: And I think the lesson that runs through all of
- 15:23Speaker 2: this research is that quality control upfront is what drives
- 15:26Speaker 2: cost effectiveness. In the long run, better materials and meticulous
- 15:30Speaker 2: prep are always cheaper than having to come back and
- 15:31Speaker 2: do it again in two years.
- 15:32Speaker 1: A perfect summary, and to really.
- 15:34Speaker 2: Drive home that idea of evaluating performance, here's a quick
- 15:37Speaker 2: exercise for you, taken right from the manual's logic. Imagine
- 15:41Speaker 2: you installed two hundred partial depth patches four years ago.
- 15:45Speaker 2: In that time, twenty of them have failed. Another five
- 15:47Speaker 2: were lost because the whole road section was rehabilitated. Your
- 15:51Speaker 2: task is to calculate the current percent patches surviving. The
- 15:54Speaker 2: formula is PS equals RIP divided by the sum of
- 15:57Speaker 2: RF plus RIP all times one hundred, where RIP as
- 16:00Speaker 2: patches in place and our FIS patches failed.
- 16:02Speaker 1: Okay, let's see, so if twenty failed and five were
- 16:04Speaker 1: loss to rehab, that leaves one hundred and seventy five
- 16:07Speaker 1: still in place. So that's one hundred and seventy five
- 16:09Speaker 1: divided by twenty failed plus one seventy five in place,
- 16:11Speaker 1: which gives you ninety point nine percent exactly ninety point
- 16:16Speaker 1: nine percent survival. If your program is hitting numbers like that,
- 16:19Speaker 1: after four years, you have the hard data to prove
- 16:22Speaker 1: that your investment in that rigorous SHRP process was worth it.
- 16:26Speaker 1: You've proven the long term value.
- 16:28Speaker 2: A fantastic practical takeaway. Apply this robust research back knowledge
- 16:32Speaker 2: to your next civil engineering challenge. Thank you for joining
- 16:35Speaker 2: us for this deep dive