Latest / Civil Engineering Made Simple / Concrete Practice
Transcript
- 0:00Speaker 1: Welcome back to the deep dive. Today. We're tackling a well,
- 0:04Speaker 1: a pretty dense topic. We're taking these massive engineering handbooks
- 0:08Speaker 1: b s N two six, STASH one and bs E
- 0:11Speaker 1: five hundred and we're going to try and boil them
- 0:13Speaker 1: down right. The goal is to distill all that technical
- 0:16Speaker 1: code into clear, usable wisdom you can actually apply on site.
- 0:21Speaker 1: We're talking about the core principles for building things that
- 0:24Speaker 1: actually last.
- 0:26Speaker 2: And they really are the rule book, aren't they. I mean,
- 0:28Speaker 2: we're talking about durability here. Concrete has been around forever,
- 0:31Speaker 2: you know, the Romans, but these standards there would allow
- 0:34Speaker 2: us to use it for everything from say critical c
- 0:38Speaker 2: defenses to the thermal mass and sustainable buildings. It's all
- 0:41Speaker 2: about sound practice.
- 0:42Speaker 1: Okay, let's get into it. The place to start has
- 0:44Speaker 1: to be the main ingredient, the binder Portland cemet or
- 0:48Speaker 1: CEMI as it's now known. But there's a whole language
- 0:51Speaker 1: around it in the standards, isn't there.
- 0:52Speaker 2: It's not just one thing, not at all. And it's
- 0:54Speaker 2: fascinating because every single bag is categorized first by its
- 0:58Speaker 2: twenty eight day strength. You'll see something like forty two
- 1:01Speaker 2: to five or fifty two five in per square millimeter,
- 1:04Speaker 2: and then by how fast it sets N for normal
- 1:08Speaker 2: early strength or R for rapid, and that difference that speed.
- 1:13Speaker 2: It's all down to the chemical recipe inside, right.
- 1:16Speaker 1: I've seen the shorthands C three S, C two S,
- 1:19Speaker 1: C three A for you know, for the learner out there,
- 1:21Speaker 1: why should they care about those letters?
- 1:23Speaker 2: You should care because that tells you how the performance
- 1:25Speaker 2: has been dialed in. So C three s that's tricalcium silicate.
- 1:29Speaker 2: It hardens really fast and gives off a lot of heat.
- 1:32Speaker 1: Okay, so that's your R type cements.
- 1:34Speaker 2: It's for a rapid hardener. Yeah. C twos, on the
- 1:36Speaker 2: other hand, is the slow and steady worker. It's responsible
- 1:39Speaker 2: for that long term strength gain. So when you pick
- 1:42Speaker 2: a fifty two thousand and five R, you're basically choosing
- 1:45Speaker 2: a mix with more C three s to hit its
- 1:47Speaker 2: strength faster.
- 1:48Speaker 1: Which is great for deadlines, but maybe not so great
- 1:50Speaker 1: for a huge thick foundation.
- 1:52Speaker 2: For exactly that heat can become a real problem. And
- 1:55Speaker 2: that leads right into this specialized cements. If you're pouring
- 1:58Speaker 2: foundations in say aggressive ground with.
- 2:00Speaker 1: Sulfates, you have to plan for that from the start.
- 2:02Speaker 2: You have to that's what sulfate resisting Portland cement or
- 2:05Speaker 2: SRPC is for. They manufacture it with really strict limits
- 2:09Speaker 2: on that fast reacting C three A compound to resist
- 2:12Speaker 2: the chemical attack. But I have to stress the cement
- 2:15Speaker 2: type is only one part of the equation. Real durability
- 2:20Speaker 2: comes from the impermeability of the finished concrete, how dense
- 2:23Speaker 2: it is.
- 2:24Speaker 1: Which brings us to additions like PIFA and GBS. These
- 2:27Speaker 1: aren't just fillers, are they. They're actually engineering the mix.
- 2:30Speaker 2: They're critical pulverized fuel ash and ground granulated blastphorous slag.
- 2:36Speaker 2: They react much slower than pure cem is cement.
- 2:39Speaker 1: Okay, and what does that slower reaction do for you?
- 2:41Speaker 2: Two really important things. First, it massively reduces the early
- 2:44Speaker 2: heat of hydration. For a big thick raft foundation, that
- 2:48Speaker 2: reduction is what stops it from cracking under its own
- 2:50Speaker 2: thermal stress.
- 2:51Speaker 1: And the second thing the long term upside.
- 2:53Speaker 2: They give you better ultimate impermeability and higher long term strength.
- 2:57Speaker 2: But and this is the crucial trade off on.
- 2:59Speaker 1: Site, there's always a trade off always.
- 3:01Speaker 2: Because they react slower, you need to cure them for
- 3:04Speaker 2: much longer, and they're way more sensitive to cold weather.
- 3:07Speaker 2: When they're first hardening. You can't rush them.
- 3:09Speaker 1: So if that's the binder, what about the bulk The aggregates.
- 3:12Speaker 1: The sand and stone make up what's seventy five percent
- 3:15Speaker 1: of the mix at least.
- 3:16Speaker 2: And the quality control there is just as demanding. They
- 3:19Speaker 2: have to be clean, I mean totally free from organic material, clay, silt,
- 3:26Speaker 2: all that stuff just ruins the wind. But ironically you
- 3:29Speaker 2: can also oversh them. If you washway too many of
- 3:32Speaker 2: the fines, the tiny particles under three hundred microns, the
- 3:35Speaker 2: mix loses its cohesion, you get more bleed water, so
- 3:38Speaker 2: it becomes unworkable. We typically use a twenty mili max
- 3:41Speaker 2: size for reinforced concrete. What about managing the stockpiles on site, specifically, the.
- 3:46Speaker 1: Moisture moisture uniformity is everything, and sand is the biggest problem.
- 3:50Speaker 1: It's moisture content can be all over them. Yeah, so
- 3:53Speaker 1: the rule of fun is to let a new sand
- 3:54Speaker 1: stockpile stand for at least twelve hours. It lets the
- 3:57Speaker 1: moisture content stabilize, usually somewhere around five seven percent. If
- 4:01Speaker 1: you don't, your batch consistency is gone. And one thing
- 4:03Speaker 1: that is an absolute non negotiable for reinforced concrete is
- 4:07Speaker 1: using marine aggregates.
- 4:09Speaker 2: Oh, absolutely, Chlorides from seawater are just a one way
- 4:12Speaker 2: ticket to steal corrosion. If you have to use marine
- 4:15Speaker 2: dredged aggregates for any concrete with metal in it, they
- 4:18Speaker 2: have to be washed rigorously, rigorously with fresh water to
- 4:22Speaker 2: meet these incredibly strict limits for reinforced concrete. With CEMI,
- 4:27Speaker 2: it's something like a maximum of point zero eight percent
- 4:30Speaker 2: chloride ion by mass. The standards are crystal clear on that.
- 4:34Speaker 1: Okay, let's switch to water. In all the literature, the
- 4:37Speaker 1: free water cement ratio is always highlighted as the single
- 4:40Speaker 1: most critical factor. How do you explain that to someone new?
- 4:43Speaker 2: I think of it as the density control knob for
- 4:45Speaker 2: the concrete. You need a certain amount of water for
- 4:48Speaker 2: the chemical reaction for hydration, but any water left over
- 4:51Speaker 2: after that reaction, any free water, just evaporates and leaves
- 4:54Speaker 2: behind a network of piny voids or capillaries.
- 4:57Speaker 1: So a high water cement ratio, say point eight, leaves
- 5:00Speaker 1: you with something like a sponge exactly.
- 5:02Speaker 2: It's porous, full of pathways for water and chemicals to
- 5:06Speaker 2: get in and attack the steel. A low ratio LIKEO
- 5:09Speaker 2: point four means the cement particles are packed really tightly.
- 5:13Speaker 2: The final product is dense, almost like rock. That's what
- 5:17Speaker 2: gives you strength and impermeability.
- 5:18Speaker 1: We know drinking water is okay to use. What's absolutely off.
- 5:22Speaker 2: Limits well seawater, as we just said, prohibited in any
- 5:26Speaker 2: concrete with embedded metal period Now. Large batching plants often
- 5:31Speaker 2: use recycled water from washing out the trucks.
- 5:33Speaker 1: M which sounds efficient.
- 5:35Speaker 2: It is, but the catch is it needs to be
- 5:37Speaker 2: filtered properly. If you're accidentally reintroducing old ad mixtures or
- 5:42Speaker 2: too many fine particles from the wash water, you're changing
- 5:44Speaker 2: the properties to the next batch without even knowing it.
- 5:47Speaker 1: And because that sand moisture is always changing, the batcher
- 5:50Speaker 1: has to constantly adjust the amount of added water to
- 5:52Speaker 1: hit that target free water summit ratio.
- 5:54Speaker 2: It's a constant balancing act. A really experienced operator can
- 5:58Speaker 2: watch the amter on the mixer motor. If the mix
- 6:01Speaker 2: gets stiffer, the motor works harder, draws more.
- 6:03Speaker 1: Current, and that tells them they need to adjust the
- 6:05Speaker 1: water instantly.
- 6:06Speaker 2: It's a skill.
- 6:07Speaker 1: So to get more precise control, we turn to chemical admixtures.
- 6:12Speaker 1: Let's start with the most common ones plasticizers.
- 6:15Speaker 2: Right, or normal water reducers. They basically lubricate the mix
- 6:19Speaker 2: at a microscopic level. They let you achieve the same
- 6:22Speaker 2: workability or slump with up to ten percent less water.
- 6:26Speaker 1: Which means you can lower your water cement ratio and
- 6:28Speaker 1: get stronger, more durable concrete. Precisely, then you have the
- 6:32Speaker 1: opposites accelerators and retarders. I know there's a big warning
- 6:36Speaker 1: with accelerators, a huge one.
- 6:38Speaker 2: They're great for speeding up strength gain and cold weather,
- 6:41Speaker 2: but any accelerator containing chlorides is absolutely forbidden and reinforced.
- 6:46Speaker 1: Concrete because of the corrosion risks.
- 6:48Speaker 2: And another key point, they are not any freeze They
- 6:51Speaker 2: just make the highgation happen faster. They don't stop the
- 6:54Speaker 2: water from freezing if it gets too cold. Retarders do
- 6:57Speaker 2: the opposite. They slow everything downel in hot weather to
- 7:00Speaker 2: stop the concrete from setting in the truck.
- 7:03Speaker 1: But there's one admixture that you just can't skip for
- 7:06Speaker 1: certain applications, and that's air and training agents. Why would
- 7:09Speaker 1: you want to add air?
- 7:10Speaker 2: It seems counterintuitive, right, you're adding bubbles.
- 7:13Speaker 1: Yeah, you're sacrificing some strength, you are?
- 7:15Speaker 2: You lose about five percent compressive strength for every one
- 7:19Speaker 2: percent of air you add. But it's a critical trade off.
- 7:22Speaker 2: Those tiny stable bubbles act as little pressure relief chambers.
- 7:26Speaker 2: When water in the concrete freezes and expands.
- 7:28Speaker 1: The bubbles give it somewhere to go and it stops.
- 7:31Speaker 2: The concrete from just shattering from the inside out. For
- 7:33Speaker 2: any external paving that will see frost, a minimum air
- 7:37Speaker 2: content of say three point five percent is non negotiable.
- 7:40Speaker 2: The durability gain is massive.
- 7:42Speaker 1: And at the high tech end we have superplasticizers. What's
- 7:46Speaker 1: the biggest risk with those on site?
- 7:48Speaker 2: So superplasticizers are high range water reducers. You can either
- 7:52Speaker 2: use them to create ultra high strength concrete or you
- 7:54Speaker 2: can create flowing, self compacting concrete.
- 7:57Speaker 1: The stuff that looks like a liquid, and that's the risk.
- 7:59Speaker 2: It behaves like liquid. It exerts full hydrostatic pressure on
- 8:02Speaker 2: your form work. If your form work isn't designed for that,
- 8:05Speaker 2: you are looking at a catastrophic failure, a blowout.
- 8:08Speaker 1: Okay, let's shift from ingredients to specifying the final product.
- 8:12Speaker 1: Strength is defined by its class, like C thirty thirty
- 8:15Speaker 1: seven measured at twenty eight days on lab cubes. But
- 8:19Speaker 1: what if you have to test the concrete that's already
- 8:21Speaker 1: in the structure.
- 8:22Speaker 2: You take core samples, and it's so important for people
- 8:25Speaker 2: to understand that a core test result will always be
- 8:28Speaker 2: lower than the result from a perfect labcured cube.
- 8:32Speaker 1: Why is that.
- 8:33Speaker 2: It's not because the concrete is necessarily bad. It's because
- 8:36Speaker 2: the drilling process itself damages the core slightly and there
- 8:39Speaker 2: are shape effects. Engineers have to account for that difference
- 8:43Speaker 2: when they're assessing if the structure is compliant.
- 8:45Speaker 1: As we've been saying, the ultimate goal is in permeability.
- 8:48Speaker 1: To manage that risk, we have the exposure classification system.
- 8:52Speaker 2: The X codes. Yes, this is really the heart of
- 8:54Speaker 2: modern durability design. It links the environment the concrete will
- 8:57Speaker 2: live in directly to the mix you need.
- 8:59Speaker 1: So it give us a few examples.
- 9:00Speaker 2: Okay, so you've got XC for carbonation risk, XSS for seawater,
- 9:04Speaker 2: and XD for other chlorides like de icing salts. XF
- 9:07Speaker 2: is for freeze though XA is for chemical attack.
- 9:10Speaker 1: And as the number goes up, say from XF one
- 9:12Speaker 1: to X four, the environment is getting harsher.
- 9:15Speaker 2: Exactly, and the standards respond by demanding a lower maximum
- 9:20Speaker 2: water hoovement ratio, a higher minimum cement content, basically forcing
- 9:24Speaker 2: you to specify a denser, more resistant concrete to cope
- 9:28Speaker 2: with that specific threat.
- 9:30Speaker 1: And what about one of the scariest long term problems
- 9:32Speaker 1: ASR alkali silica reaction.
- 9:35Speaker 2: Concrete cancer as some people call it. It's insidious. You
- 9:38Speaker 2: need three things to happen at once for it to start.
- 9:40Speaker 2: You use a certain type of reactive silica in your aggregate,
- 9:43Speaker 2: high alkalinity in the cement paste, and you need moisture.
- 9:47Speaker 2: Take away any one of those three and ASR can't happen.
- 9:50Speaker 1: And this is another reason people use things like PIFA
- 9:52Speaker 1: or ggb's.
- 9:53Speaker 2: It's a major reason. They effectively dilute the alkalinity of
- 9:57Speaker 2: the mix, removing one of those essential triggers for their reaction.
- 10:01Speaker 1: So once the engineer has figured all this out, how
- 10:03Speaker 1: do they actually order the concrete? We hear terms like designed,
- 10:06Speaker 1: prescribed and designated.
- 10:08Speaker 2: Right, So if you order a design mix, you specify
- 10:11Speaker 2: the performance you need. You say I need C thirty
- 10:13Speaker 2: EREAR thirty seven strength, a max water summit ratio OFERO
- 10:16Speaker 2: point five, and the supplier designs the mix to meet.
- 10:18Speaker 1: That and you prove it works with strength tests. You do.
- 10:21Speaker 2: But if you order a standardized prescribed mix like an STMX.
- 10:26Speaker 2: You're specifying the recipe itself. You're saying, I want these
- 10:29Speaker 2: exact proportions. Conformity there is checked by looking at the
- 10:32Speaker 2: supplier's batch records, not usually by routine strength testing on site.
- 10:37Speaker 1: Let's get to the sharpened site execution. You can have
- 10:41Speaker 1: the best mix in the world, but if you place
- 10:43Speaker 1: it badly, it's all wasted.
- 10:45Speaker 2: The golden rule is to place it as close as
- 10:47Speaker 2: possible to its final position.
- 10:49Speaker 1: You don't just dump it in one corner and push it.
- 10:51Speaker 2: Around these don't never ever use the poker vibrator to
- 10:55Speaker 2: move concrete horizontally. That just causes segregation. The heavy stones
- 11:00Speaker 2: uprates from the paste and you're left with a weak,
- 11:02Speaker 2: non uniform mess. Place it in layers maybe five hundred
- 11:05Speaker 2: mil thick max.
- 11:06Speaker 1: And compaction is obviously non negotiable. What does good vibration
- 11:09Speaker 1: technique look like.
- 11:10Speaker 2: It's about getting the entrapped air out. Just one percent
- 11:13Speaker 2: of leftover air voids can knock over five percent off
- 11:15Speaker 2: your final strength. It's huge. So the technique you insert
- 11:19Speaker 2: the poker vibrator quickly, make sure it goes into the
- 11:21Speaker 2: layer below by about one hundred mil to stitch the
- 11:23Speaker 2: two layers together and then you pull it out slowly.
- 11:27Speaker 2: When the air bubbles stop rising to the surface, your
- 11:30Speaker 2: job is done. Move to the next spot.
- 11:32Speaker 1: Is it ever a good idea to revibrate concrete after
- 11:35Speaker 1: it's been compacted.
- 11:36Speaker 2: Yes, Ashley, it's a really useful technique as long as
- 11:40Speaker 2: the concrete is still plastic, still workable.
- 11:42Speaker 1: What's the benefit.
- 11:44Speaker 2: It's great for clothing up any of those little plastic
- 11:46Speaker 2: settlement cracks that can form on the surface, and it
- 11:49Speaker 2: can actually improve the bond to the reinforcement.
- 11:51Speaker 1: Now, what about construction joints where fresh concrete meets a
- 11:55Speaker 1: pore from yesterday.
- 11:57Speaker 2: The keyword there is bond. You need a good bond
- 12:00Speaker 2: and you can't get that if there's a layer of
- 12:02Speaker 2: latens on the old surface.
- 12:03Speaker 1: Layton's being that weak, milky layer of cement that rises
- 12:07Speaker 1: to the top.
- 12:07Speaker 2: That's the stuff. The best way to deal with it
- 12:10Speaker 2: is to remove it when the concrete is still green,
- 12:12Speaker 2: just a few hours old. A sift brush and a
- 12:14Speaker 2: light spray of water will do it. If it's already hard,
- 12:17Speaker 2: you have to use a wire brush or mechanically scalbleet.
- 12:20Speaker 2: And crucially don't paint the joint with a grout or
- 12:23Speaker 2: mortar before you pour. The research shows it doesn't really
- 12:27Speaker 2: help the bond strength.
- 12:29Speaker 1: Last big topic then curing. Why is it so important
- 12:32Speaker 1: to stop the surface drying out in those first few days.
- 12:35Speaker 2: Curing is all about keeping the water in so the
- 12:38Speaker 2: hydration reaction can continue. This is especially vital for the
- 12:41Speaker 2: surface zone. The cover concrete that protects your steel.
- 12:45Speaker 1: That's your first line of defense.
- 12:47Speaker 2: It's everything. If that cover is weak and porous because
- 12:49Speaker 2: it dried out too fast, carbonation and chlorides will get
- 12:52Speaker 2: to your steel much quicker.
- 12:53Speaker 1: So what are the minimum times.
- 12:55Speaker 2: For a standard cemi mix in average weather? You're looking
- 12:58Speaker 2: at a minimum of seven days for a horizontal slab,
- 13:01Speaker 2: maybe three days for a vertical wall. And if you've
- 13:04Speaker 2: used we fo or jigads, you need to extend those.
- 13:06Speaker 1: Times because of that slower reaction exactly. And a final
- 13:10Speaker 1: quick word on extreme weather cold and hot.
- 13:12Speaker 2: Okay, cold weather, the concrete must be above five degree
- 13:16Speaker 2: c when you place it. If you need to heat
- 13:18Speaker 2: the mix, heat the water before you add the cement,
- 13:20Speaker 2: otherwise you can get a flash set. And hot weather,
- 13:23Speaker 2: the risk is rapid water loss and stiffening You can
- 13:27Speaker 2: use retarders to slow things down, but the absolute number
- 13:30Speaker 2: one warning is never retemper meaning never add more water
- 13:34Speaker 2: to a mix that has started to stiffen just to
- 13:36Speaker 2: make it workable again, you have just destroyed the water
- 13:40Speaker 2: sment made ratio. That batch has to be rejected.
- 13:42Speaker 1: So we've gone from the chemistry of cement all the
- 13:45Speaker 1: way to how to treat a construction joint. It seems
- 13:48Speaker 1: like the two things that come up again and again
- 13:49Speaker 1: are controlling that free water sment ratio and then just
- 13:53Speaker 1: diligent execution on site.
- 13:55Speaker 2: That's it. That's the foundation of good practice. So what
- 13:58Speaker 2: for you, the listener, is that you can now see
- 14:00Speaker 2: beyond just a simple slump test. You understand the compromises
- 14:04Speaker 2: like trading early strengths for long term durability, and that
- 14:08Speaker 2: knowledge is what helps you spot a risk on site
- 14:11Speaker 2: before it becomes a failure.
- 14:12Speaker 1: Okay, to wrap this up, here's a short exercise for you,
- 14:15Speaker 1: the future site leader, to really lock this in. A
- 14:18Speaker 1: ready mixed trick shows up on a hot, windy day.
- 14:21Speaker 1: The ticket says see three way three seven concrete max
- 14:24Speaker 1: free water SMIT ratio of point five zero. You do
- 14:27Speaker 1: a slump test and it's too stiff. The driver offers
- 14:30Speaker 1: to add twenty liters of water to get it to
- 14:32Speaker 1: the right consistency. What is your immediate course of action
- 14:36Speaker 1: and why.
- 14:37Speaker 2: Your immediate course of action has to be to refuse
- 14:39Speaker 2: the water and reject the load and reject the load?
- 14:41Speaker 1: Why so absolutely, Because.
- 14:43Speaker 2: The second you add that unmeasured water, the free water,
- 14:45Speaker 2: some ratio goes above that point five zero maximum specified
- 14:49Speaker 2: for durability. You've just compromised the entire structure.
- 14:51Speaker 1: You've opened up those capillary voids we talked about you have.
- 14:54Speaker 2: You've increased its permeability, you've reduced its resistance to chlorides
- 14:58Speaker 2: and carbonation, and you viole the fundamental specification. Sacrificing that
- 15:02Speaker 2: long term durability just for a bit of temporary workability
- 15:05Speaker 2: is never an option.
- 15:06Speaker 1: Sound practice keeps structure standing. Go out there and apply
- 15:10Speaker 1: these key nuggets of knowledge.