- 0:00Speaker 1: Welcome back to the deep dive. Today, we are getting
- 0:02Speaker 1: into the weeds on a standard that is absolutely foundational
- 0:06Speaker 1: for seismic fabrication quality. We're talking about AWSD ON one
- 0:10Speaker 1: ten eight D one point aim twenty twenty one, the
- 0:13Speaker 1: Structural Welding Code Seismic Supplement. Now, if you're an engineer,
- 0:17Speaker 1: a fabricator, an inspector, really anyone touching steel structures in
- 0:22Speaker 1: a seismic region, this isn't just another codebook. It's the
- 0:25Speaker 1: playbook for ensuring a building can actually withstand an earthquake.
- 0:28Speaker 1: So our mission today is to give you that practical
- 0:31Speaker 1: operational roadmap. We want to get to the why behind
- 0:34Speaker 1: the rules.
- 0:35Speaker 2: The why is everything, and it's really rooted in some
- 0:37Speaker 2: hard won lessons from history. I mean, D one point
- 0:39Speaker 2: eight came about largely because of the failures we saw
- 0:42Speaker 2: in welded steel moment frame buildings during the nineteen ninety
- 0:45Speaker 2: four North Rage earthquake. Engineers, you know, they had designed
- 0:48Speaker 2: these connections with the idea that the steel beams would yield,
- 0:51Speaker 2: that they would absorb all that seismic energy, the concept
- 0:53Speaker 2: of ductility.
- 0:54Speaker 1: Like a metal sponge basically exactly.
- 0:56Speaker 2: But that's not what happened. What happened was the welds themselves,
- 0:59Speaker 2: the part everyone assumed for the strongest link. They just
- 1:02Speaker 2: fractured cleanly.
- 1:03Speaker 1: A brittle failure, a.
- 1:04Speaker 2: Catastrophic brittle failure. The energy absorption mechanism just failed. The
- 1:09Speaker 2: buildings didn't bend, they broke.
- 1:11Speaker 1: So aws D one point one is the baseline for
- 1:14Speaker 1: all structural welding. But D one point eight steps in
- 1:16Speaker 1: and says, hold on a minute. For these specific joints,
- 1:20Speaker 1: the ones that have to endure this incredible strain, we
- 1:24Speaker 1: need a whole other level of quality control.
- 1:26Speaker 2: That's it, precisely. D one point eight applies when you're
- 1:28Speaker 2: using the AISC seismic provisions. It doesn't replace D one
- 1:32Speaker 2: point one. It supplements it. It layers on much much
- 1:36Speaker 2: stricter rules for your materials, for the welding process, for
- 1:39Speaker 2: the welders themselves, and of course for inspection.
- 1:41Speaker 1: Okay, so let's start with the language. Before we can
- 1:43Speaker 1: apply the rules, we have to know where to apply them.
- 1:46Speaker 1: What are the key terms that define the scope here.
- 1:48Speaker 2: Well, the broadest term is the seismic force resisting system
- 1:51Speaker 2: or SFRS. Yeah, this is basically the structural skeleton. The
- 1:54Speaker 2: beams columns, the connections that the engineer is designated to
- 1:57Speaker 2: take the seismic hit. But not every weld in the
- 2:01Speaker 2: SFRS gets the D one point eight treatment.
- 2:03Speaker 1: You have to narrow it down, which brings us to
- 2:05Speaker 1: I think the most important term here, the protected zone.
- 2:08Speaker 2: The protected zone. Yes, this is the specific spot on
- 2:12Speaker 2: a beam or column where the engineer expects plastic hinging
- 2:16Speaker 2: to happen. It's where the yielding is supposed to occur.
- 2:19Speaker 1: So that's the real AHA moment for me. It's not
- 2:21Speaker 1: a weakness, it's a designed feature. It's where you've given
- 2:24Speaker 1: the building permission to bend so it doesn't break somewhere else.
- 2:28Speaker 2: That's a perfect way to put it. And because it's
- 2:30Speaker 2: so critical. D one point eight is incredibly strict about it.
- 2:34Speaker 2: You can't just go drilling holes in it or making
- 2:36Speaker 2: temporary attachment.
- 2:37Speaker 1: You can't compromise its ability to stretch.
- 2:39Speaker 2: You can't, not without explicit approval.
- 2:43Speaker 1: So that brings us to the third term, demand critical
- 2:46Speaker 1: welds or DC welds. These are the specific welds that
- 2:50Speaker 1: the engineer calls out, usually the ones connecting elements inside
- 2:53Speaker 1: that protected zone. Think of the big groove welds. Joining
- 2:56Speaker 1: a beam flange to a column.
- 2:57Speaker 2: And when a weld gets that DC label, that's the trigger.
- 3:01Speaker 1: That's the trigger. It immediately kicks in the highest level
- 3:04Speaker 1: of scrutiny. In D one point eight special filler Metal,
- 3:06Speaker 1: Special procedures, you name it, it's the code basically saying
- 3:10Speaker 1: this weld cannot be the weaklink, got it and.
- 3:12Speaker 2: The last one the last one is lowest anticipated service
- 3:16Speaker 2: temperature or st The engineer establishes this and it has
- 3:21Speaker 2: a huge impact on material selection.
- 3:23Speaker 1: Why does the coldest day the building will ever see
- 3:25Speaker 1: matter so much for the welds.
- 3:27Speaker 2: Because steals behavior changes with temperature. A metal that's nice
- 3:31Speaker 2: and tough at room temperature can become brittle when it
- 3:33Speaker 2: gets cold. The magic number in D one point eight
- 3:37Speaker 2: is fifty degrees fahrenheit or ten celsius. If you're all
- 3:41Speaker 2: last is at or above that, you follow one set
- 3:44Speaker 2: of rules for toughness testing. If it's below that, the
- 3:47Speaker 2: requirements get even tougher. Literally, that makes a lot of sense.
- 3:51Speaker 1: So once we've identified a demand critical weld, we have
- 3:55Speaker 1: to look at materials and procedures. And it's not just
- 3:57Speaker 1: about strength anymore, is it. It's all about toughness.
- 4:00Speaker 2: It's all about toughness. For the filler metals used in
- 4:02Speaker 2: DC wells, the strength is high, sure, but the real
- 4:05Speaker 2: star of the show is the CVN toughness. The code
- 4:08Speaker 2: demands a minimum of forty foot pounds of energy absorption
- 4:11Speaker 2: at seventy degrees fahrenheit.
- 4:13Speaker 1: Okay, forty foot pounds. Unpack that for us? What does
- 4:15Speaker 1: that number actually mean and why is it so important?
- 4:18Speaker 2: CVN or chirpy V notch testing is essentially a measure
- 4:22Speaker 2: of a material's resistance to crack propagation. Think of toughness
- 4:26Speaker 2: as as the ability to absorb energy before fracturing. If
- 4:30Speaker 2: a tiny crack forms in that weld, a high toughness
- 4:33Speaker 2: means it takes a huge amount of energy at forty
- 4:36Speaker 2: foot pounds to make that crack grow. It ensures the
- 4:39Speaker 2: steel yields first.
- 4:40Speaker 1: So it buys you time for the ductility to kick
- 4:42Speaker 1: in precisely.
- 4:43Speaker 2: And to maintain that toughness, you have to control the
- 4:45Speaker 2: welding process itself, which is where the heat input envelope
- 4:48Speaker 2: from ANNEXA comes in. You can't just grab any old
- 4:50Speaker 2: D one point one procedure. Why not?
- 4:52Speaker 1: What is heat input? Due to that toughness.
- 4:54Speaker 2: Too much heat is the enemy of toughness. Very high
- 4:57Speaker 2: heat input can change the microstructure of the well. It
- 5:00Speaker 2: makes the grains courser, and that just kills your notch toughness.
- 5:03Speaker 2: You can completely undo all the good properties of that
- 5:06Speaker 2: expensive filler metal. So NXA makes you qualify your procedure
- 5:10Speaker 2: both ends of the spectrum. You run one test at
- 5:12Speaker 2: a low heat input and another at a very high heat.
- 5:14Speaker 1: Input, creating a window an envelope.
- 5:17Speaker 2: Exactly, you create an envelope and you have to prove
- 5:20Speaker 2: that the weld is tough enough at both the low
- 5:23Speaker 2: and high end. Then in production, all your welding has
- 5:27Speaker 2: to stay within that qualified range. It's a fantastic process control.
- 5:31Speaker 1: It's an engineered range, not just a recipe. What about
- 5:34Speaker 1: other factors? I know hydrogen is a big one. Oh.
- 5:36Speaker 2: Hydrogen is the invisible enemy. It can lead to delayed cracking,
- 5:39Speaker 2: especially in these massive, highly restrained joints. So D one
- 5:42Speaker 2: point eight is very clear. All electrodes and fluxes have
- 5:45Speaker 2: to be low hydrogen. Specifically, they must meet an H
- 5:49Speaker 2: sixteen maximum, which is sixteen milli liters per one hundred grams.
- 5:53Speaker 2: You need the paperwork to prove it.
- 5:54Speaker 1: And what about mixing different welding processes in one joint.
- 5:57Speaker 1: I've heard there are special rules for self shield at
- 6:00Speaker 1: flux cored arc welding.
- 6:01Speaker 2: Yes FCAWS. Yeah, self shielded is unique because it uses
- 6:05Speaker 2: a lot of chemical deoxidizers and its flux core instead
- 6:09Speaker 2: of a shielding gas and put a layer of say,
- 6:11Speaker 2: stick weld on top of a cell shielded weld. The
- 6:13Speaker 2: chemistries can interact in a bad way. It's been shown
- 6:16Speaker 2: to cause a sudden, unexpected drop in toughness.
- 6:18Speaker 1: So you have to test them together.
- 6:19Speaker 2: You have to ANNEXB requires a specific intermixed CVN test
- 6:24Speaker 2: to prove that the combination of processes still meets that
- 6:29Speaker 2: forty foot pound requirement. It's a critical safety check.
- 6:32Speaker 1: Okay, that's a great overview of the material site. Now
- 6:34Speaker 1: let's talk about the physical details the geometry, because Northridge
- 6:39Speaker 1: taught us that sharp corners are basically fracture starting points.
- 6:42Speaker 2: They are, and that lesson starts with what's called the
- 6:45Speaker 2: K area. The K area right, it's that little spot
- 6:48Speaker 2: on a steel beam or column web right next to
- 6:50Speaker 2: where the flange is connected. During the milling process the
- 6:53Speaker 2: steel mill, this area gets.
- 6:55Speaker 1: Cold worked so it's already stressed and has lower toughness
- 6:58Speaker 1: before you even start welding it. It's like a built
- 7:00Speaker 1: in weak spot.
- 7:01Speaker 2: It's the steal's achilles heel exactly. So if you weld
- 7:04Speaker 2: a stiffer plate right up into that corner, you're putting
- 7:06Speaker 2: a massive stress riser right on top of an already
- 7:09Speaker 2: vulnerable area. D one point eight forbids that it requires
- 7:13Speaker 2: those plates to be clipped. You have to physically cut
- 7:15Speaker 2: the corner of the plate off so that the welld
- 7:17Speaker 2: terminates at least an inch and a half away from
- 7:19Speaker 2: that sensitive K area.
- 7:21Speaker 1: Such a small detail, but it prevents a massive potential failure.
- 7:25Speaker 1: What about backing bars another classic problem.
- 7:28Speaker 2: Area, a huge one for the critical beam bottom flange weld.
- 7:31Speaker 2: D one point eight generally says the steel backing has
- 7:34Speaker 2: to come off. Then you have to gouge the root
- 7:36Speaker 2: out to clean metal fill it. And this is the
- 7:39Speaker 2: key part. At a minimum five hundred and sixteen inch
- 7:42Speaker 2: reinforcing fill a weld.
- 7:44Speaker 1: And that filet isn't for strength, is it?
- 7:46Speaker 2: No? Not really, it's for geometry. It smooths out that
- 7:49Speaker 2: sharp ninety degree corner where the beam, the column and
- 7:52Speaker 2: the weld all meet. It just eases the stress flow.
- 7:55Speaker 1: And if you're allowed to leave the backing in place,
- 7:57Speaker 1: say on the top flange.
- 7:59Speaker 2: Same principle apply. You have to add that same five
- 8:01Speaker 2: hundred and sixteen inch filo weld, but this time it
- 8:04Speaker 2: connects the backing bar to the column face. And this
- 8:07Speaker 2: is a huge inspection item. You are absolutely forbidden from
- 8:10Speaker 2: welding the backing bar to the underside of the bean
- 8:13Speaker 2: flange that creates the exact kind of notch D one
- 8:15Speaker 2: point eight is trying to eliminate.
- 8:16Speaker 1: Okay, So the level of detail here is incredible, which
- 8:19Speaker 1: means the people doing the work and checking the work
- 8:21Speaker 1: have to be a cut above two they do.
- 8:24Speaker 2: D one point eight singles out one weld as being
- 8:26Speaker 2: the toughest that bottom beam flange groove weld made through
- 8:30Speaker 2: the little access hole in the beam web.
- 8:32Speaker 1: The access is just terrible.
- 8:34Speaker 2: It's awful. And because of that, D one point eight
- 8:37Speaker 2: requires a special supplemental welder qualification, which is detailed in NXD.
- 8:42Speaker 1: So this is on top of their normal D one
- 8:44Speaker 1: point one.
- 8:45Speaker 2: Qualification on top of it. Yes, it's a restricted access
- 8:48Speaker 2: welding test. It's a performance test to prove that a
- 8:50Speaker 2: welder can actually produce a sound weld in that incredibly cramped,
- 8:54Speaker 2: difficult position, and that qualification is only good for thirty six.
- 8:58Speaker 1: Months, A key thing for any quality manager to track.
- 9:01Speaker 1: What about the inspectors NDT technicians.
- 9:04Speaker 2: So your QA inspector needs to be a CWI, But
- 9:07Speaker 2: for the ultrasonic testing or UT technicians, D one point
- 9:10Speaker 2: eight raises the bar significantly. They have to be a
- 9:13Speaker 2: certified Level two or three. But then they also have
- 9:15Speaker 2: to pass a special practical exam described in ANNEXF.
- 9:19Speaker 1: A practical exam. How's that different from a standard UT certification?
- 9:22Speaker 2: This is a hands on test. They give the technician
- 9:25Speaker 2: mockup blocks that have real known flaws welded into them, cracks,
- 9:30Speaker 2: lack of fusion, you name it, and the tech is
- 9:32Speaker 2: graded on their ability to find, locate, and correctly size
- 9:35Speaker 2: those flaws. The passing grade is extremely high. It proves
- 9:39Speaker 2: they can do the job in practice, not just on paper. Wow.
- 9:42Speaker 1: Okay, and let's circle back one last time to that
- 9:44Speaker 1: vulnerable K area. There's a very specific timing rule for
- 9:47Speaker 1: inspecting it isn't there.
- 9:49Speaker 2: This might be one of the most important and most
- 9:51Speaker 2: frequently missed rules in the entire code. The forty eight hour.
- 9:54Speaker 1: Delay A forty eight hour delay.
- 9:56Speaker 2: Yes, after you've welded a continuity plate or a doubler
- 9:59Speaker 2: plate to a co you must perform magnetic particle testing
- 10:02Speaker 2: MPT on that K area base metal. But you cannot
- 10:05Speaker 2: do it any sooner than forty eight hours after the
- 10:07Speaker 2: welding is finished.
- 10:08Speaker 1: Why why the two day weight.
- 10:10Speaker 2: It's because of delayed hydrogen cragging. That failure mechanism, which
- 10:14Speaker 2: is common in that cold work to zone, doesn't happen instantly.
- 10:18Speaker 2: The hydrogen needs time to migrate, The stresses need time
- 10:21Speaker 2: to build up. The crack might not even exist one
- 10:23Speaker 2: hour after welding, but it could be there thirty six
- 10:26Speaker 2: hours later. If you inspect too soon, you get a
- 10:29Speaker 2: false negative. The forty eight hour weight is mandatory insurance
- 10:32Speaker 2: against that.
- 10:33Speaker 1: That one rule could completely change the production schedule on
- 10:37Speaker 1: a job. So trap this up D one point eight
- 10:39Speaker 1: isn't just a set of arbitrary rules. It's a complete
- 10:41Speaker 1: system designed to build ductility into a welded connection. We've
- 10:45Speaker 1: talked about controlling the materials properties with CVN and hydrogen limits,
- 10:48Speaker 1: controlling the process with the heat input envelope, and controlling
- 10:51Speaker 1: the geometry by eliminating those dangerous notches.
- 10:54Speaker 2: It's exactly and for anyone listening. If you're a young engineer,
- 10:58Speaker 2: a new inspector, you have to have these things on
- 11:01Speaker 2: your radar. Know what a DC weld designation means, know
- 11:05Speaker 2: about the supplemental welder qualification, and please remember that forty
- 11:09Speaker 2: hour delay on the K area. These details define a
- 11:12Speaker 2: successful seismic project. To help you put this all together,
- 11:15Speaker 2: here's a little exercise. Imagine you are the QA inspector
- 11:18Speaker 2: on a moment frame job. A welder just finished the
- 11:20Speaker 2: CJ